Powder Coating tip

fingers284

CGN Ultra frequent flyer
Rating - 100%
4   0   0
Just read a tip on the "other boolit site" that I don't know how I missed as it was first posted in early summer.

It seems that someone in the "hi humidity" belt down south noticed that if you are having trouble getting good powder coverage with the swirl method that a pre-swirl of 40 or 50 seconds with only the powder and no bullets in the tub yet will pre-charge the static needed for better 'stick-ability" of the powder. Some are claiming larger batches of bullets can be swirled in each tub full by doing this as well.

So if your first venture into powder coating left a little to be desired this may remedy the issue, I haven't tried it yet as I'm still setting up my new casting station and all my boolit coating stuff hasn't been taken out for the winter use season yet...

Good luck
 