Tempilaq 750

ffgats

CGN frequent flyer
Rating - 100%
99   0   0
Hi, I know reloaders put Tempilq inside the neck, hardly noticed when the its start to melt or change colour, what do you think if applied to the shoulder instead at the neck shoulder area. Thanks
 
Interesting. Since I like to remain open minded, when it comes to different techniques...I will have to try some testing on the inside of the neck.
Could be very useful information.
 
Inside the neck on 223. It was pretty clear to me when it melted away. I made sure to have good lighting.
 
it should be applied inside the case neck, putting it on the outside probably results in an incorrect result from direct flame. I wouldn't apply a big blob of it on the inside either, just enough to get a good read and easy to clean out after the job is done.
 
I use it inside. I use cases that are scrap to test the flame with so I don't mess good ones. The Tempilaq goes to flame just before the case drops out of the torch flame.
 
I will be buying the 700 Tempilaq for easier setup, zinc melts around 780F, so maybe the 700 is safer not to melt zinc, any comments?, thanks
 
Back