Hi everyone!
I have a general question about harness. I got the lee tester and everything i test seem to be realy smooter than what i should expect.
My lyman #2 made from 9pound of WW and one pound of tin babbitt turn around 10 BHN and should be at 15.
My 20 to 1 alloy turn around 8.2 BHN and should be at 10.
what are your experience with alloy and tester? and can some of you can tell me how hard they get with those alloy?
Have a great day all'z
I have a general question about harness. I got the lee tester and everything i test seem to be realy smooter than what i should expect.
My lyman #2 made from 9pound of WW and one pound of tin babbitt turn around 10 BHN and should be at 15.
My 20 to 1 alloy turn around 8.2 BHN and should be at 10.
what are your experience with alloy and tester? and can some of you can tell me how hard they get with those alloy?
Have a great day all'z