- Location
- Iroquois Falls ON
Info that came with my Lee mold says that a 10 to 1 mix of lead and tin should be good for my .44 Russian. As I have both in pure ingots I would like to make use of them.
Is that mix by volume or weight?
Thanks
Is that mix by volume or weight?
Thanks