Just finished annealing 75 cases for my 7mm Weatherby mag. 58 are Weatherby brass, 17 are federal 7mm rem mag.
Bucket of water, propane torch, and my fingers to hold and spin the cases. 11 seconds in the flame to get the "dull red" in my darkened bathroom. Pretty easy actually, didn't even burn my fingers. The cases now look like factory Lapua brass I have seen images of on the intrawebs.
I thought this post would be longer, but that about covers it.
Bucket of water, propane torch, and my fingers to hold and spin the cases. 11 seconds in the flame to get the "dull red" in my darkened bathroom. Pretty easy actually, didn't even burn my fingers. The cases now look like factory Lapua brass I have seen images of on the intrawebs.
I thought this post would be longer, but that about covers it.