I had an older gentleman stop into the shop today wondering if we could refinish an Anshutz Model 470 rifle he had purchased. I was unsure what the receiver material was made of so I couldn't give a sure answer.
Does anyone know what material the receivers were made of?
I'm guessing it is a zinc based die casting as it was nonmagnetic yet too heavy to be aluminum. If so, anyone have success anodizing zinc based castings? I told him I'd look into it and get back to him. Hopefully you guys can help me out.