When some one says add some flux to clean up the melt, what does one use and how much say in a 10lb melt.
Also when you add 2% tin (using lead free solder) is that 2% weight of solder compared to weight of lead, so again assuming you have 10lb pure lead =160oz would you add about 3.2 oz of solder to get the right hardness for smokeless loads?