Here we go...
The standard Canadian heat souce, a Coleman campstove. Hot water with TSP in the left bucket, and the bluing solution in the right. The SS buckets came from the Army/Navy store.
Here is a milling clamp I made a while back. It is cold rolled steel.
This is O-1 tool steel. It turned out slightly red.
These threaded rod were cold rolled steel. They turned out super dark blue.
The standard Canadian heat souce, a Coleman campstove. Hot water with TSP in the left bucket, and the bluing solution in the right. The SS buckets came from the Army/Navy store.
Here is a milling clamp I made a while back. It is cold rolled steel.
This is O-1 tool steel. It turned out slightly red.
These threaded rod were cold rolled steel. They turned out super dark blue.
Last edited: