I used Lee Liquid Alox for my cast .38 (.360) Bullets. It was used without any thinning, but it's still sticky after 2 days. Is this normal?
Also does anyone have a recipe for .38 S&W using HS6? Bullet is LEE TL358-158-2R. dopping from the mold nicely at .360.
I've done many percentage difference calculations between other powders and the HS6 would seem to need 3 - 3.4 grains. But I have no proven safe recipe.
Also does anyone have a recipe for .38 S&W using HS6? Bullet is LEE TL358-158-2R. dopping from the mold nicely at .360.