Hornady used to make hydro forming dies, may still. They simply do not form the casings as well as COW method does. Both are messy processes, 1 has cream of wheat with a funky smell all over the place, the other has water everywhere.
Of the 2 processes I have found the COW method to be far superior. YMMV