Going to try some FFg or FFFg in a couple of 38-55's. I read that this powder is not as corrosive as there is no sulphur in it, but then also read best practice is to treat and clean everything as though it is corrosive? Whats the best way to treat things?
Default is always 'do the most' but why waste steps
Have tried a couple rounds and then cleaned as per normal routine and 1st patches were black but cleared up quick
Hope to take the rifle to a BP shoot coming up that will allow some easing of the normal stiff BP-only rules.
Default is always 'do the most' but why waste steps
Have tried a couple rounds and then cleaned as per normal routine and 1st patches were black but cleared up quick
Hope to take the rifle to a BP shoot coming up that will allow some easing of the normal stiff BP-only rules.