1954 Russian SKS -- laminate stock refinished in tung oil

I just rubbed it with 0000 wool before last coat(#6), wiped down with a clean cotton rag. Then gave it a nice coat of tung oil and did not wipe it off after the 20 min, then let it sit for over 30 hrs. Leave it and walk away. I did not use wax.
It came to a nice hard coat.....buffed it with a cotton rag and here it is........................ tried it out on my chinese....I will more than likely install this on my 1950 Tula.

P1000295.jpg

Nice work!! Well done.
 
Dang those are looking nice. Quick q though.. Are you guys putting on a wax of some sort as a last stage, and if so, what kind?

I put some stain on mine and 6 coats of tung oil and am just wondering if it's done lol. It looks great so far but just worried I'm skipping a step.
Thanks

I will give it the occasional wipe down with a Hoppe's cloth (silicone treated).
However, wax is not really necessary.
 