I have read that once the final pass is complete to soak parts in oil for a week. Some say to soak using USED motor oil, others say clean gun oil.
What's the recommendation from those in the know? Is there any benefit in leaving parts soak in a warm environment to let the blue "set"?
I've done a rust blue before and the results were great. Some say 5-7 passes but I went for 3 on a project with good results. One article mentioned the fewer passes the better as the result is a shinier patina (vs. more of a matte blue for increasing passes). Any thoughts?
What's the recommendation from those in the know? Is there any benefit in leaving parts soak in a warm environment to let the blue "set"?
I've done a rust blue before and the results were great. Some say 5-7 passes but I went for 3 on a project with good results. One article mentioned the fewer passes the better as the result is a shinier patina (vs. more of a matte blue for increasing passes). Any thoughts?
Last edited: